CONCRETE SLAB THICKNESS
09-20-2010, 02:25 PM
Post: #3
RE: CONCRETE SLAB THICKNESS
Well, I guess I just ask! I check the prints, look for cored holes, cut-outs at HVAC shafts, whatever, but I need to rely on the owner or General's knowledge of how thick the slab is.

That said, there is always risk that the slab isn't what they think it is! Multiple tests will help show discrepancies, so watch for those. Poured in place slabs or even poured-in-pan can vary several inches in thickness from edge to center. Your probes will show patterned variations usually.

I document the thickness and note that the testing is done at 'X' depth, based on the GC / Owner's statement of exiting conditions. If they tell me the slab is 4" thick and it's really 14", well whose fault is it that I am only in 1.6" now?

And believe me this can and does happen!

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com
Find all posts by this user
Quote this message in a reply
Post Reply 


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious

Messages In This Thread
CONCRETE SLAB THICKNESS - MINUS - 09-02-2010, 09:48 AM
RE: CONCRETE SLAB THICKNESS - Ernesto - 09-03-2010, 08:13 AM
RE: CONCRETE SLAB THICKNESS - CC Solutions - 09-20-2010 02:25 PM