Thanks Jim, I was gonna blow a fuse if someone was telling you that somehow moisture content correlates to RH. We've had discussions on this forum for years regarding that very issue.
And besides, the Tramex should always be used as a qualitative measuring tool, never a quantitative one. ![]() Yes Pat, that seems like many moons ago when you first came to us, all bright and shiny and ready to add your input. What a great contributor you have been!! ![]() How are things on the flip side of the planet? What do you guys think about Iran and Israel and all the world news? We're going to war soon... are you in?
JD Grafton Concrete Answers for Flooring Problems JGrafton@ccsolves.com |
|||
|
« Next Oldest | Next Newest »
|
![]() |
|||||||
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
|
| Messages In This Thread |
|
Bad, Bad Testing - CCR - 12-18-2012, 02:35 PM
RE: Bad, Bad Testing - Rubensgt40 - 12-18-2012, 08:15 PM
RE: Bad, Bad Testing - CCR - 12-19-2012, 05:20 AM
RE: Bad, Bad Testing - Rubensgt40 - 12-19-2012, 03:07 PM
RE: Bad, Bad Testing - CCR - 12-19-2012, 04:00 PM
RE: Bad, Bad Testing - CC Solutions - 12-20-2012, 08:09 PM
RE: Bad, Bad Testing - CCR - 12-20-2012, 08:34 PM
RE: Bad, Bad Testing - CC Solutions - 12-20-2012, 09:32 PM
RE: Bad, Bad Testing - eaadams - 12-22-2012, 12:24 PM
RE: Bad, Bad Testing - CCR - 12-22-2012, 01:02 PM
RE: Bad, Bad Testing - eaadams - 12-22-2012, 01:46 PM
RE: Bad, Bad Testing - CC Solutions - 12-22-2012, 02:54 PM
RE: Bad, Bad Testing - eaadams - 12-23-2012, 11:50 AM
RE: Bad, Bad Testing - CCR - 12-23-2012, 12:30 PM
RE: Bad, Bad Testing - Rubensgt40 - 12-29-2012, 04:43 AM
RE: Bad, Bad Testing - CC Solutions - 12-29-2012, 10:26 PM
RE: Bad, Bad Testing - Rubensgt40 - 12-30-2012, 06:30 PM
RE: Bad, Bad Testing - CC Solutions - 12-30-2012, 06:45 PM
RE: Bad, Bad Testing - CCR - 01-03-2013, 10:36 AM
RE: Bad, Bad Testing - jim decker - 03-21-2013, 08:41 AM
RE: Bad, Bad Testing - CC Solutions - 03-21-2013, 12:02 PM
RE: Bad, Bad Testing - jim decker - 03-21-2013, 01:26 PM
RE: Bad, Bad Testing - CC Solutions - 03-21-2013, 02:48 PM
RE: Bad, Bad Testing - jim decker - 03-21-2013, 03:31 PM
RE: Bad, Bad Testing - Rubensgt40 - 03-21-2013, 06:29 PM
RE: Bad, Bad Testing - CC Solutions - 03-21-2013 06:58 PM
RE: Bad, Bad Testing - Rubensgt40 - 03-21-2013, 07:47 PM
RE: Bad, Bad Testing - CC Solutions - 03-22-2013, 03:28 AM
RE: Bad, Bad Testing - hausenheimer - 03-24-2013, 06:06 AM
RE: Bad, Bad Testing - CCR - 03-24-2013, 06:40 AM
RE: Bad, Bad Testing - Rubensgt40 - 03-24-2013, 04:13 PM
RE: Bad, Bad Testing - CC Solutions - 03-25-2013, 05:43 AM
RE: Bad, Bad Testing - hausenheimer - 03-28-2013, 08:45 AM
|



Help
Advanced Search




![[-] [-]](images/collapse.gif)