slab warmer than air
|
|
01-24-2013, 05:50 PM
Post: #1
|
|||
|
|||
|
slab warmer than air
Here is a first. Slab is warmer than the air. (it has been colder than average in California) RH results should be lower right?
2" slab on Bitumin layer on 6" slab on an old cemetery (so they don't want to remove the slab for fear of the un-dead! har har har) |
|||
|
01-24-2013, 07:03 PM
Post: #2
|
|||
|
|||
|
RE: slab warmer than air
Well, yeah, all things being equal the warmer air inside the slab would mean a lower %.
But if there's zombies involved, all things are not equal. Pat Atherton Floor Test Australia www.moisturetesting.com.au "Democracy ... can only exist until the majority discover they can vote themselves largess out of the public treasury" - Tytler, De Tocqueville, Reagan |
|||
|