is there " White Paper " out there on RH Testing of Pre Cast that is covered by self leveling.
|
|||
|
01-24-2013, 05:05 PM
Post: #2
|
|||
|
|||
|
RE: Pre Cast / Self Leveling
Not that I'm aware of. Why would you want to test AFTER the self-leveler is installed? All testing should be done BEFORE any topping, skimcoat or self-leveler is installed because moisture mitigation systems should be installed directly over ther affected concrete. There are a couple of MM products that claim they can be installed over self-levelers but I'm not so sure that's a good thing. And until I see it for myself, I simply don't believe it.
JK Nixon Concrete Restoration Services, LLC Pittsburgh, PA http://www.rhtester.com |
|||
|