Pre Cast / Self Leveling
01-21-2013, 11:45 AM
Post: #1
Pre Cast / Self Leveling
is there " White Paper " out there on RH Testing of Pre Cast that is covered by self leveling.
Find all posts by this user
Quote this message in a reply
01-24-2013, 05:05 PM
Post: #2
RE: Pre Cast / Self Leveling
Not that I'm aware of. Why would you want to test AFTER the self-leveler is installed? All testing should be done BEFORE any topping, skimcoat or self-leveler is installed because moisture mitigation systems should be installed directly over ther affected concrete. There are a couple of MM products that claim they can be installed over self-levelers but I'm not so sure that's a good thing. And until I see it for myself, I simply don't believe it.

JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com
Visit this user's website Find all posts by this user
Quote this message in a reply
Yesterday, 01:31 PM
Post: #3
RE: Pre Cast / Self Leveling
I have a job that has structural plank with a 3" cement based topping over it, can RH testing be performed to verify the moisture content of the topping? I have attached the mix specifications with page 1 being the topping over the plank.


Attached File(s)
.pdf  topping and concrete mixes.pdf (Size: 134.18 KB / Downloads: 4)
Find all posts by this user
Quote this message in a reply
Today, 09:57 AM
Post: #4
RE: Pre Cast / Self Leveling
A cement based topping is not a self leveling underlayment.

Self Leveling Underlayments (ardex K-15 or equal) are entirely a different animal from what you are working with.