12-30-2012, 06:45 PM
Post: #18
RE: Bad, Bad Testing
I am sure this happens Mr. R... The GC laments that he cannot finish his building on time and will suffer huge economic loss due to delays because he cannot install his vinyl flooring on 6th floor!

Well whadayaknow? For a cool couple hundred bucks, maybe a grand, XYZ is showing the floors PASS and the work can continue!!!

Oh happy day until there is a problem.... Sad

Then there are installers who will install vinyl even when I show them the floor is at 95%. When I asked one company owner how he could possibly do that he told me he has a one year warranty so he will come back for the first year and fix any bubbles but after that he is GONE....

I almost called the building owner on that one. The flooring company and the GC were screwing over a VERY large hospital by installing a vinyl flooring on very wet slabs... About 30,000 square feet of it.....

Who polices this stuff?

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com
Find all posts by this user
Quote this message in a reply
Post Reply 


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious

Messages In This Thread
Bad, Bad Testing - CCR - 12-18-2012, 02:35 PM
RE: Bad, Bad Testing - Rubensgt40 - 12-18-2012, 08:15 PM
RE: Bad, Bad Testing - CCR - 12-19-2012, 05:20 AM
RE: Bad, Bad Testing - Rubensgt40 - 12-19-2012, 03:07 PM
RE: Bad, Bad Testing - CCR - 12-19-2012, 04:00 PM
RE: Bad, Bad Testing - CC Solutions - 12-20-2012, 08:09 PM
RE: Bad, Bad Testing - CCR - 12-20-2012, 08:34 PM
RE: Bad, Bad Testing - CC Solutions - 12-20-2012, 09:32 PM
RE: Bad, Bad Testing - eaadams - 12-22-2012, 12:24 PM
RE: Bad, Bad Testing - CCR - 12-22-2012, 01:02 PM
RE: Bad, Bad Testing - eaadams - 12-22-2012, 01:46 PM
RE: Bad, Bad Testing - CC Solutions - 12-22-2012, 02:54 PM
RE: Bad, Bad Testing - eaadams - 12-23-2012, 11:50 AM
RE: Bad, Bad Testing - CCR - 12-23-2012, 12:30 PM
RE: Bad, Bad Testing - Rubensgt40 - 12-29-2012, 04:43 AM
RE: Bad, Bad Testing - CC Solutions - 12-29-2012, 10:26 PM
RE: Bad, Bad Testing - Rubensgt40 - 12-30-2012, 06:30 PM
RE: Bad, Bad Testing - CC Solutions - 12-30-2012 06:45 PM
RE: Bad, Bad Testing - CCR - 01-03-2013, 10:36 AM
RE: Bad, Bad Testing - jim decker - 03-21-2013, 08:41 AM
RE: Bad, Bad Testing - CC Solutions - 03-21-2013, 12:02 PM
RE: Bad, Bad Testing - jim decker - 03-21-2013, 01:26 PM
RE: Bad, Bad Testing - CC Solutions - 03-21-2013, 02:48 PM
RE: Bad, Bad Testing - jim decker - 03-21-2013, 03:31 PM
RE: Bad, Bad Testing - Rubensgt40 - 03-21-2013, 06:29 PM
RE: Bad, Bad Testing - CC Solutions - 03-21-2013, 06:58 PM
RE: Bad, Bad Testing - Rubensgt40 - 03-21-2013, 07:47 PM
RE: Bad, Bad Testing - CC Solutions - 03-22-2013, 03:28 AM
RE: Bad, Bad Testing - hausenheimer - 03-24-2013, 06:06 AM
RE: Bad, Bad Testing - CCR - 03-24-2013, 06:40 AM
RE: Bad, Bad Testing - Rubensgt40 - 03-24-2013, 04:13 PM
RE: Bad, Bad Testing - CC Solutions - 03-25-2013, 05:43 AM
RE: Bad, Bad Testing - hausenheimer - 03-28-2013, 08:45 AM