Event: 12/6 CSI Topic: Floor Slab Moisture
|
|
12-22-2012, 04:15 PM
Post: #16
|
|||
|
|||
|
RE: Event: 12/6 CSI Topic: Floor Slab Moisture
In California I see it on >90% of jobs. At least every week. It may be cut and paste / lazy specs. When I confront the engineers on it, it is usually in hopes of lessening for slab curl since the prices people get for grinding off some curled edges are outrageous.
I see it most often in the Dessert from Cal and down through Arizona. |
|||
|