Cork flooring
|
|
12-21-2012, 07:20 AM
Post: #21
|
|||
|
|||
|
RE: Cork flooring
Glad everyone likes it. I love the stuff!!! Installed pretty easy?
JK Nixon Concrete Restoration Services, LLC Pittsburgh, PA http://www.rhtester.com |
|||
|
12-21-2012, 08:40 AM
Post: #22
|
|||
|
|||
|
RE: Cork flooring
Installation was a snap... Literally!
The plank cork was a bit tighter, I think the bigger size pieces in the office were not as tight on one edge. There always seemed to be a hairline crack in the same point of each tile joint. The planks are amazingly tight, the manufacturer must have some impressive machinery making these products to install so tightly. JD Grafton Concrete Answers for Flooring Problems JGrafton@ccsolves.com |
|||
|
12-21-2012, 09:11 AM
Post: #23
|
|||
|
|||
|
RE: Cork flooring
Who was the manufacturer?
JK Nixon Concrete Restoration Services, LLC Pittsburgh, PA http://www.rhtester.com |
|||
|
12-21-2012, 10:05 AM
Post: #24
|
|||
|
|||
|
RE: Cork flooring
Wicanders made the flooring...
JD Grafton Concrete Answers for Flooring Problems JGrafton@ccsolves.com |
|||
|
12-22-2012, 11:49 AM
Post: #25
|
|||
|
|||
|
RE: Cork flooring
any all details & pictures would be cool
|
|||
|
12-22-2012, 03:07 PM
Post: #26
|
|||
|
|||
|
RE: Cork flooring
I will... Give me some time... I have to get trim on and all that stuff!
JD Grafton Concrete Answers for Flooring Problems JGrafton@ccsolves.com |
|||
|
04-29-2013, 08:36 PM
Post: #27
|
|||
|
|||
|
RE: Cork flooring
Cork is a great floor do a lot of US Floors never a problem. Years ago when I did all of Dartmouth Colleges floor work in NH. I replaced a cork floor in the administration building that had been down 50 years didn't look bad replaced with nylon commercial carpet.
Beware of click wood or cork if the house cannot maintain the relative humidity requirements of the cork mfg. Particularly in arid areas if they shrink somewhat as they then may make clicking noises. |
|||
|