To be candid, I and a handful of others have an interest in seeing some kind of industry drive towards testing by independent (certified) agencies.

That said, it's still simply the best common sense approach and hopefully the industry will eventually push it. We know the wheels turn slowly in this regard but it's encouraging to know that independent agencies are currently getting some work anyway. I'm all set up and ready to go, but haven't yet gone out into the big wide world of marketing the service, and I'm blessed with gainful employment in the meantime.

Equally, there's nothing wrong with mitigation specialists like JD being responsible for testing. There's no "vested interest" other than seeing that flooring doesn't fail. It still safeguards against the Builder/ GC/ Installer-invoked pressure to rush installation.

What worries me is that, if it takes a long time to get the message across in the US, how long will it take here!

Pat Atherton
Floor Test Australia
www.moisturetesting.com.au

"Democracy ... can only exist until the majority discover they can vote themselves largess out of the public treasury" - Tytler, De Tocqueville, Reagan
Find all posts by this user
Quote this message in a reply
Post Reply 


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious

Messages In This Thread
Bad, Bad Testing - CCR - 12-18-2012, 02:35 PM
RE: Bad, Bad Testing - Rubensgt40 - 12-18-2012, 08:15 PM
RE: Bad, Bad Testing - CCR - 12-19-2012, 05:20 AM
RE: Bad, Bad Testing - Rubensgt40 - 12-19-2012 03:07 PM
RE: Bad, Bad Testing - CCR - 12-19-2012, 04:00 PM
RE: Bad, Bad Testing - CC Solutions - 12-20-2012, 08:09 PM
RE: Bad, Bad Testing - CCR - 12-20-2012, 08:34 PM
RE: Bad, Bad Testing - CC Solutions - 12-20-2012, 09:32 PM
RE: Bad, Bad Testing - eaadams - 12-22-2012, 12:24 PM
RE: Bad, Bad Testing - CCR - 12-22-2012, 01:02 PM
RE: Bad, Bad Testing - eaadams - 12-22-2012, 01:46 PM
RE: Bad, Bad Testing - CC Solutions - 12-22-2012, 02:54 PM
RE: Bad, Bad Testing - eaadams - 12-23-2012, 11:50 AM
RE: Bad, Bad Testing - CCR - 12-23-2012, 12:30 PM
RE: Bad, Bad Testing - Rubensgt40 - 12-29-2012, 04:43 AM
RE: Bad, Bad Testing - CC Solutions - 12-29-2012, 10:26 PM
RE: Bad, Bad Testing - Rubensgt40 - 12-30-2012, 06:30 PM
RE: Bad, Bad Testing - CC Solutions - 12-30-2012, 06:45 PM
RE: Bad, Bad Testing - CCR - 01-03-2013, 10:36 AM
RE: Bad, Bad Testing - jim decker - 03-21-2013, 08:41 AM
RE: Bad, Bad Testing - CC Solutions - 03-21-2013, 12:02 PM
RE: Bad, Bad Testing - jim decker - 03-21-2013, 01:26 PM
RE: Bad, Bad Testing - CC Solutions - 03-21-2013, 02:48 PM
RE: Bad, Bad Testing - jim decker - 03-21-2013, 03:31 PM
RE: Bad, Bad Testing - Rubensgt40 - 03-21-2013, 06:29 PM
RE: Bad, Bad Testing - CC Solutions - 03-21-2013, 06:58 PM
RE: Bad, Bad Testing - Rubensgt40 - 03-21-2013, 07:47 PM
RE: Bad, Bad Testing - CC Solutions - 03-22-2013, 03:28 AM
RE: Bad, Bad Testing - hausenheimer - 03-24-2013, 06:06 AM
RE: Bad, Bad Testing - CCR - 03-24-2013, 06:40 AM
RE: Bad, Bad Testing - Rubensgt40 - 03-24-2013, 04:13 PM
RE: Bad, Bad Testing - CC Solutions - 03-25-2013, 05:43 AM
RE: Bad, Bad Testing - hausenheimer - 03-28-2013, 08:45 AM