Bad Sensor
12-07-2012, 07:13 PM
Post: #60
RE: Bad Sensor
I believe with E-96 they knew what they wanted to test for, and then used the product they felt would give the best results.

With 1869, it started by dumping some salt on a slab and seeing if it got wet. If it did the slab failed, if it didn't the slab passed. They didn't use cups or hoods or weighed samples for a long time! So what were they looking for? What water amount was going to be acceptable? What time period to let the calcium absorb? This was all just made up as they went along.

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com
Find all posts by this user
Quote this message in a reply
Post Reply 


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious

Messages In This Thread
Bad Sensor - Ernesto - 11-07-2012, 04:36 PM
RE: Bad Sensor - rapidrhrep - 11-07-2012, 07:46 PM
RE: Bad Sensor - Ernesto - 11-08-2012, 07:16 AM
RE: Bad Sensor - rapidrhrep - 11-08-2012, 10:55 AM
RE: Bad Sensor - Rubensgt40 - 11-08-2012, 05:56 PM
RE: Bad Sensor - Ernesto - 11-08-2012, 08:30 PM
RE: Bad Sensor - rapidrhrep - 11-08-2012, 10:44 PM
RE: Bad Sensor - Ernesto - 11-09-2012, 06:33 PM
RE: Bad Sensor - Rubensgt40 - 11-10-2012, 01:11 AM
RE: Bad Sensor - Ernesto - 11-10-2012, 08:43 AM
RE: Bad Sensor - CC Solutions - 11-15-2012, 02:37 PM
RE: Bad Sensor - Ernesto - 11-15-2012, 04:09 PM
RE: Bad Sensor - CC Solutions - 11-15-2012, 06:02 PM
RE: Bad Sensor - Ernesto - 11-15-2012, 07:51 PM
RE: Bad Sensor - CC Solutions - 11-15-2012, 09:49 PM
RE: Bad Sensor - Ernesto - 11-16-2012, 06:51 AM
RE: Bad Sensor - Rubensgt40 - 11-21-2012, 05:35 PM
RE: Bad Sensor - CC Solutions - 11-21-2012, 08:14 PM
RE: Bad Sensor - CCR - 11-22-2012, 06:50 AM
RE: Bad Sensor - Ernesto - 11-22-2012, 09:31 AM
RE: Bad Sensor - Rubensgt40 - 11-22-2012, 06:03 PM
RE: Bad Sensor - CCR - 11-23-2012, 11:51 AM
RE: Bad Sensor - Ernesto - 11-24-2012, 09:14 AM
RE: Bad Sensor - CCR - 11-25-2012, 07:17 AM
RE: Bad Sensor - Ernesto - 11-26-2012, 09:25 AM
RE: Bad Sensor - rapidrhrep - 11-26-2012, 03:50 PM
RE: Bad Sensor - CC Solutions - 11-26-2012, 04:32 PM
RE: Bad Sensor - Rubensgt40 - 11-26-2012, 06:57 PM
RE: Bad Sensor - CC Solutions - 11-26-2012, 09:07 PM
RE: Bad Sensor - eaadams - 11-27-2012, 09:14 AM
RE: Bad Sensor - Ernesto - 11-27-2012, 02:00 PM
RE: Bad Sensor - Ernesto - 11-27-2012, 03:33 PM
RE: Bad Sensor - CCR - 11-27-2012, 05:27 PM
RE: Bad Sensor - Ernesto - 11-27-2012, 06:22 PM
RE: Bad Sensor - rapidrhrep - 11-28-2012, 09:58 AM
RE: Bad Sensor - Ernesto - 11-28-2012, 10:06 AM
RE: Bad Sensor - surfacesteve - 11-30-2012, 09:53 AM
RE: Bad Sensor - Ernesto - 11-30-2012, 05:09 PM
RE: Bad Sensor - eaadams - 11-30-2012, 05:33 PM
RE: Bad Sensor - CC Solutions - 12-01-2012, 08:24 AM
RE: Bad Sensor - Ernesto - 12-01-2012, 05:18 PM
RE: Bad Sensor - CC Solutions - 12-01-2012, 06:44 PM
RE: Bad Sensor - Ernesto - 12-03-2012, 06:48 PM
RE: Bad Sensor - Rubensgt40 - 12-03-2012, 06:59 PM
RE: Bad Sensor - Ernesto - 12-04-2012, 07:57 AM
RE: Bad Sensor - CC Solutions - 12-04-2012, 10:38 AM
RE: Bad Sensor - Ernesto - 12-04-2012, 08:28 PM
RE: Bad Sensor - CC Solutions - 12-05-2012, 07:23 AM
RE: Bad Sensor - CCR - 12-05-2012, 08:00 AM
RE: Bad Sensor - CC Solutions - 12-05-2012, 08:35 AM
RE: Bad Sensor - CCR - 12-05-2012, 08:45 AM
RE: Bad Sensor - CC Solutions - 12-05-2012, 09:54 AM
RE: Bad Sensor - CCR - 12-05-2012, 12:05 PM
RE: Bad Sensor - CC Solutions - 12-05-2012, 12:58 PM
RE: Bad Sensor - Ernesto - 12-06-2012, 06:41 PM
RE: Bad Sensor - CCR - 12-07-2012, 04:36 AM
RE: Bad Sensor - Ernesto - 12-07-2012, 07:24 AM
RE: Bad Sensor - CC Solutions - 12-07-2012, 07:32 AM
RE: Bad Sensor - Ernesto - 12-07-2012, 06:44 PM
RE: Bad Sensor - CC Solutions - 12-07-2012 07:13 PM
RE: Bad Sensor - Ernesto - 12-08-2012, 08:32 AM
RE: Bad Sensor - Ernesto - 12-10-2012, 04:48 PM