The 'pedigree' has nothing to do with the test itself. It has to do with the numbers being used. Who decided that 3lbs, or 5 lbs is good? And why? And who decided how to prep the slab? Clean it? Grind it? Sand it? 24 hour open period? 20"x20" square? Why? And why did it all change? And what exactly did the change do?
There was never a scientific process to the test. It started with putting CaCl granules on the floor and covering it with a plastic sheet and seeing if the CaCl granules got wet. THAT was the basis of the test. Very arbitrary. JD Grafton Concrete Answers for Flooring Problems JGrafton@ccsolves.com |
|||
|
« Next Oldest | Next Newest »
|
![]() |
|||||||
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
|
| Messages In This Thread |
|
Bad Sensor - Ernesto - 11-07-2012, 04:36 PM
RE: Bad Sensor - rapidrhrep - 11-07-2012, 07:46 PM
RE: Bad Sensor - Ernesto - 11-08-2012, 07:16 AM
RE: Bad Sensor - rapidrhrep - 11-08-2012, 10:55 AM
RE: Bad Sensor - Rubensgt40 - 11-08-2012, 05:56 PM
RE: Bad Sensor - Ernesto - 11-08-2012, 08:30 PM
RE: Bad Sensor - rapidrhrep - 11-08-2012, 10:44 PM
RE: Bad Sensor - Ernesto - 11-09-2012, 06:33 PM
RE: Bad Sensor - Rubensgt40 - 11-10-2012, 01:11 AM
RE: Bad Sensor - Ernesto - 11-10-2012, 08:43 AM
RE: Bad Sensor - CC Solutions - 11-15-2012, 02:37 PM
RE: Bad Sensor - Ernesto - 11-15-2012, 04:09 PM
RE: Bad Sensor - CC Solutions - 11-15-2012, 06:02 PM
RE: Bad Sensor - Ernesto - 11-15-2012, 07:51 PM
RE: Bad Sensor - CC Solutions - 11-15-2012, 09:49 PM
RE: Bad Sensor - Ernesto - 11-16-2012, 06:51 AM
RE: Bad Sensor - Rubensgt40 - 11-21-2012, 05:35 PM
RE: Bad Sensor - CC Solutions - 11-21-2012, 08:14 PM
RE: Bad Sensor - CCR - 11-22-2012, 06:50 AM
RE: Bad Sensor - Ernesto - 11-22-2012, 09:31 AM
RE: Bad Sensor - Rubensgt40 - 11-22-2012, 06:03 PM
RE: Bad Sensor - CCR - 11-23-2012, 11:51 AM
RE: Bad Sensor - Ernesto - 11-24-2012, 09:14 AM
RE: Bad Sensor - CCR - 11-25-2012, 07:17 AM
RE: Bad Sensor - Ernesto - 11-26-2012, 09:25 AM
RE: Bad Sensor - rapidrhrep - 11-26-2012, 03:50 PM
RE: Bad Sensor - CC Solutions - 11-26-2012, 04:32 PM
RE: Bad Sensor - Rubensgt40 - 11-26-2012, 06:57 PM
RE: Bad Sensor - CC Solutions - 11-26-2012, 09:07 PM
RE: Bad Sensor - eaadams - 11-27-2012, 09:14 AM
RE: Bad Sensor - Ernesto - 11-27-2012, 02:00 PM
RE: Bad Sensor - Ernesto - 11-27-2012, 03:33 PM
RE: Bad Sensor - CCR - 11-27-2012, 05:27 PM
RE: Bad Sensor - Ernesto - 11-27-2012, 06:22 PM
RE: Bad Sensor - rapidrhrep - 11-28-2012, 09:58 AM
RE: Bad Sensor - Ernesto - 11-28-2012, 10:06 AM
RE: Bad Sensor - surfacesteve - 11-30-2012, 09:53 AM
RE: Bad Sensor - Ernesto - 11-30-2012, 05:09 PM
RE: Bad Sensor - eaadams - 11-30-2012, 05:33 PM
RE: Bad Sensor - CC Solutions - 12-01-2012, 08:24 AM
RE: Bad Sensor - Ernesto - 12-01-2012, 05:18 PM
RE: Bad Sensor - CC Solutions - 12-01-2012, 06:44 PM
RE: Bad Sensor - Ernesto - 12-03-2012, 06:48 PM
RE: Bad Sensor - Rubensgt40 - 12-03-2012, 06:59 PM
RE: Bad Sensor - Ernesto - 12-04-2012, 07:57 AM
RE: Bad Sensor - CC Solutions - 12-04-2012, 10:38 AM
RE: Bad Sensor - Ernesto - 12-04-2012, 08:28 PM
RE: Bad Sensor - CC Solutions - 12-05-2012, 07:23 AM
RE: Bad Sensor - CCR - 12-05-2012, 08:00 AM
RE: Bad Sensor - CC Solutions - 12-05-2012, 08:35 AM
RE: Bad Sensor - CCR - 12-05-2012, 08:45 AM
RE: Bad Sensor - CC Solutions - 12-05-2012, 09:54 AM
RE: Bad Sensor - CCR - 12-05-2012, 12:05 PM
RE: Bad Sensor - CC Solutions - 12-05-2012, 12:58 PM
RE: Bad Sensor - Ernesto - 12-06-2012, 06:41 PM
RE: Bad Sensor - CCR - 12-07-2012, 04:36 AM
RE: Bad Sensor - Ernesto - 12-07-2012, 07:24 AM
RE: Bad Sensor - CC Solutions - 12-07-2012 07:32 AM
RE: Bad Sensor - Ernesto - 12-07-2012, 06:44 PM
RE: Bad Sensor - CC Solutions - 12-07-2012, 07:13 PM
RE: Bad Sensor - Ernesto - 12-08-2012, 08:32 AM
RE: Bad Sensor - Ernesto - 12-10-2012, 04:48 PM
|



Help
Advanced Search



![[-] [-]](images/collapse.gif)