measurement in a cold slab
|
|
12-04-2012, 02:45 PM
Post: #1
|
|||
|
|||
|
measurement in a cold slab
Hello All, my first time using the rapidRH on a concrete slab. The RH came back as 90% rh at 51 deg F. We were planning to coat this floor with epoxy. The building is on top of a hill and on all sides the terrain is slopped down and away. The heat is turned down since they are not currently
using it. Is there a correction I can apply to my readings to correct for the cold conditions. Thanks |
|||
|
« Next Oldest | Next Newest »
|
![]() |
|||||||
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
|
| Messages In This Thread |
|
measurement in a cold slab - Noweare - 12-04-2012 02:45 PM
RE: measurement in a cold slab - CCR - 12-05-2012, 05:47 AM
RE: measurement in a cold slab - CC Solutions - 12-05-2012, 07:37 AM
RE: measurement in a cold slab - Noweare - 12-05-2012, 10:59 AM
RE: measurement in a cold slab - CC Solutions - 12-05-2012, 12:55 PM
RE: measurement in a cold slab - eaadams - 12-19-2012, 01:22 PM
RE: measurement in a cold slab - CCR - 12-19-2012, 02:12 PM
RE: measurement in a cold slab - Ernesto - 12-19-2012, 03:18 PM
RE: measurement in a cold slab - eaadams - 12-19-2012, 03:19 PM
RE: measurement in a cold slab - Ernesto - 12-20-2012, 03:37 PM
RE: measurement in a cold slab - eaadams - 12-20-2012, 04:23 PM
RE: measurement in a cold slab - Ernesto - 12-20-2012, 06:23 PM
RE: measurement in a cold slab - CC Solutions - 12-20-2012, 07:55 PM
RE: measurement in a cold slab - eaadams - 12-21-2012, 04:29 PM
RE: measurement in a cold slab - eaadams - 01-18-2013, 05:02 PM
|