I watched the video as well, cept after the first time I used it. You forgot the - 11 after the advice on getting the standard.

Plus.....my instructions that came with the sensor/reader pack clearly shows a picture with the white insertion tool being used! Tongue

Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com
Visit this user's website Find all posts by this user
Quote this message in a reply
11-27-2012, 03:33 PM
Post: #32
RE: Bad Sensor
Here's some pics I just took. Why is the sensor wider than 3/4in? Big Grin



.jpg  Rapid Rh and Drill bit dimensions 062.JPG (Size: 69.16 KB / Downloads: 15)

.jpg  Rapid Rh and Drill bit dimensions 065.JPG (Size: 67.53 KB / Downloads: 13)

Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com
Visit this user's website Find all posts by this user
Quote this message in a reply
11-27-2012, 05:27 PM
Post: #33
RE: Bad Sensor
Very interesting! Although it appears the angle of the bit and blade tips are not precisely perpendicular to the gauge (?)

JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com
Visit this user's website Find all posts by this user
Quote this message in a reply
11-27-2012, 06:22 PM
Post: #34
RE: Bad Sensor
(11-27-2012 05:27 PM)CCR Wrote:  Very interesting! Although it appears the angle of the bit and blade tips are not precisely perpendicular to the gauge (?)

JK, it would seem that way but thats the widest point as the cutters/tips of the bit are angled. Take a close look at yours. If not angled they would not cut but just spin around.

Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com
Visit this user's website Find all posts by this user
Quote this message in a reply
11-28-2012, 09:58 AM
Post: #35
RE: Bad Sensor
Ernesto keep in mind you want to measure the body of the sensor, not including fins. They are there for isolation and conform to hole diameter. Had you measured the original 4.0 you would have seen the same dimensions.

Jason
Find all posts by this user
Quote this message in a reply
11-28-2012, 10:06 AM (This post was last modified: 11-28-2012 03:54 PM by Ernesto.)
Post: #36
RE: Bad Sensor
(11-28-2012 09:58 AM)rapidrhrep Wrote:  Ernesto keep in mind you want to measure the body of the sensor, not including fins. They are there for isolation and conform to hole diameter. Had you measured the original 4.0 you would have seen the same dimensions.

Jason

I realized the fins collapse somewhat to seal any malformations of the hole or what have you, but do cause some resistance if they are 1 mm wider. What my main intent was to show you I have the right bit.

But still, the glossy picture in the instruction literature showed the white insertion tool being used, and nothing about using a black insertion tool. So, as per your post about following instruction, I did. Plus there is nothing said about having to use the new black tool in the non-glossy supplemental instructions either.

Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com
Visit this user's website Find all posts by this user
Quote this message in a reply
11-30-2012, 09:53 AM
Post: #37
RE: Bad Sensor
I'm not using an insertion tool and only using the caps. However, I take my Relton bits from Wagner and have them sharpened by an industrial blade sharpening shop (even the new ones). I know some will say that you cant keep an sharp edge on a roto-bit but these guys do a great job and my sensors go in smooth and snug. Getting a perfectly round true 3/4 hole is key.

Steve Anderson
President
Surface Testing Group
Find all posts by this user
Quote this message in a reply
11-30-2012, 05:09 PM
Post: #38
RE: Bad Sensor
(11-30-2012 09:53 AM)surfacesteve Wrote:  I'm not using an insertion tool and only using the caps. However, I take my Relton bits from Wagner and have them sharpened by an industrial blade sharpening shop (even the new ones). I know some will say that you cant keep an sharp edge on a roto-bit but these guys do a great job and my sensors go in smooth and snug. Getting a perfectly round true 3/4 hole is key.

You mean you only use the cap to insert the sensor? Thats a great idea, thanks.

I'm feel abandoned by the rapidrhrep......Confused Thought thats what the forum was for. Maybe it's just for a dog an pony show. Huh

Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com
Visit this user's website Find all posts by this user
Quote this message in a reply
11-30-2012, 05:33 PM
Post: #39
RE: Bad Sensor
what is the problem again?
Find all posts by this user
Quote this message in a reply
12-01-2012, 08:24 AM
Post: #40
RE: Bad Sensor
I remember a scramble to get a black insertion tool on the market because the white one was destroying probes.

From the pictures I've seen, the black tool pushes on the sleeve so it doesn't ruin the sensor.

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com
Find all posts by this user
Quote this message in a reply
Post Reply 


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious