A most unfortunate flooring failure!
|
|
11-20-2012, 03:53 PM
Post: #14
|
|||
|
|||
|
RE: A most unfortunate flooring failure!
I'm with you. But being your own boss has more benefits in the end. And when it comes to standing behind your work for a good customer, ya do what ya gotta do.
JK Nixon Concrete Restoration Services, LLC Pittsburgh, PA http://www.rhtester.com |
|||
|
« Next Oldest | Next Newest »
|
![]() |
|||||||
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
|