A most unfortunate flooring failure!
11-19-2012, 02:34 PM
Post: #6
RE: A most unfortunate flooring failure!
I disagree. After this installer gets burned, and then sees that the testing is as easy as drilling a hole and inserting a reader, he'll be sure to use RH probes every time.

At least that is what I have noticed around here. The Rapid RH is so easy and so quick, guys that install expensive flooring are very eager to use them now.

JD Grafton
Concrete Answers for Flooring Problems