Use a proper vapor retarder directly under the slab (no blotter layer). Pour a well graded concrete mix (high strength /less cement). Limit the amount of water not just W/C ratio (you can limit cement also). Finish the concrete so it is left porous and breathes. (I have begun to add to my specs's - "perform a single steel pass to create a smooth finish, do not over finish concrete." ) Cure the concrete with water for 3 days only. Eliminate re-wetting. Promote drying with airflow and low humidity. Test the slab using Wagner Rapid RH probes. Glue directly to the concrete and enjoy. ----------------------- What would you add to this to limit curling? I know it isn't moisture but a big part of my issues with getting properly done slab on vapor membrane is limiting curling. Side note: "evil flooring spirits" gave me a great chuckle. I didn't realize I had been missing out on such a good thread. |
|||
|
« Next Oldest | Next Newest »
|
![]() |
|||||||
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
|



Help
Advanced Search



![[-] [-]](images/collapse.gif)