A most unfortunate flooring failure!
11-19-2012, 11:25 AM
Post: #3
RE: A most unfortunate flooring failure!
(11-16-2012 09:38 AM)CC Solutions Wrote:  If we would have known this slab may have had moisture problems we would have tested it before installing the flooring

aka if I thought I could win the bid and include the cost of doing $xxxx or testing I would have but I didn't because I wouldn't get the work if the other guy wan't going to do the testing.
Find all posts by this user
Quote this message in a reply
Post Reply 


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious

Messages In This Thread
RE: A most unfortunate flooring failure! - eaadams - 11-19-2012 11:25 AM