(10-11-2012 11:49 AM)lean Wrote: Hello. I just have a concrete patio done. It is cut into rectangles. Two of the rectangles got curvy and rain water stays in them. Can one replace just these two blocks? Is it difficult? Thank you Hello, If you are still looking for a solution.... Meet MG-Krete by Imco Technologies http://illianaenterprises.com/meet-mg-kr...ologies-2/ MG Krete is the best kept secret and ABSOLUTE BEST option for concrete repair and restoration. |
|||
|