RE: RH Testing Thick Slabs
(10-14-2012 09:55 AM)CC Solutions Wrote: Being that slabs dry to the top, you could drill down until you hit a point that exceeds the maximum level of RH and stop there. On the other hand, if you do not drill down to the required depth, and your reading is low, your just wasting your time and a sensor. Stephen Perrera dba Top Floor Installation Co. http://www.tucsonazflooring.com http://www.floorsavior.com |
|||
|