RH Testing Thick Slabs
09-24-2012, 06:21 PM
Post: #1
RH Testing Thick Slabs
Anyone have suggestions for testing an 18" thick slab using the Wagner Reader?

With a 40% depth of 7.2", I'm afraid the reader will be diffucult if not impossible to remove. Slab was installed over Sega vapor barrier, but it will probably never dry in my lifetime, or my son's, or grandson's.

I wonder if I even need to set the sensors that deep. Wonder if the length of the reader less 1/4" to grab onto would suffice?

JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com
Visit this user's website Find all posts by this user
Quote this message in a reply
Post Reply 


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious

Messages In This Thread
RH Testing Thick Slabs - CCR - 09-24-2012 06:21 PM
RE: RH Testing Thick Slabs - eaadams - 09-25-2012, 09:25 AM
RE: RH Testing Thick Slabs - CCR - 09-25-2012, 10:03 AM
RE: RH Testing Thick Slabs - eaadams - 09-25-2012, 10:06 AM
RE: RH Testing Thick Slabs - CCR - 09-25-2012, 10:13 AM
RE: RH Testing Thick Slabs - Rubensgt40 - 10-09-2012, 07:07 PM
RE: RH Testing Thick Slabs - CCR - 10-10-2012, 02:10 PM
RE: RH Testing Thick Slabs - Ernesto - 10-10-2012, 04:24 PM
RE: RH Testing Thick Slabs - CCR - 10-10-2012, 04:58 PM
RE: RH Testing Thick Slabs - Ernesto - 10-10-2012, 07:24 PM
RE: RH Testing Thick Slabs - CC Solutions - 10-13-2012, 08:29 PM
RE: RH Testing Thick Slabs - Ernesto - 10-14-2012, 08:19 AM
RE: RH Testing Thick Slabs - CC Solutions - 10-14-2012, 09:55 AM
RE: RH Testing Thick Slabs - Ernesto - 10-14-2012, 07:46 PM
RE: RH Testing Thick Slabs - CC Solutions - 10-15-2012, 06:07 AM
RE: RH Testing Thick Slabs - CCR - 10-17-2012, 01:07 PM
RE: RH Testing Thick Slabs - Ernesto - 10-18-2012, 08:01 PM
RE: RH Testing Thick Slabs - CCR - 10-19-2012, 05:39 AM
RE: RH Testing Thick Slabs - Ernesto - 10-19-2012, 06:41 PM
RE: RH Testing Thick Slabs - Rubensgt40 - 10-23-2012, 06:16 PM
RE: RH Testing Thick Slabs - Ernesto - 10-24-2012, 07:44 AM
RE: RH Testing Thick Slabs - rapidrhrep - 10-24-2012, 08:08 AM
RE: RH Testing Thick Slabs - CCR - 11-20-2012, 03:18 PM
RE: RH Testing Thick Slabs - CC Solutions - 11-20-2012, 03:28 PM
RE: RH Testing Thick Slabs - CCR - 11-20-2012, 03:43 PM
RE: RH Testing Thick Slabs - CC Solutions - 11-20-2012, 05:21 PM
RE: RH Testing Thick Slabs - eaadams - 11-20-2012, 05:26 PM
RE: RH Testing Thick Slabs - CC Solutions - 11-20-2012, 05:30 PM
RE: RH Testing Thick Slabs - CCR - 11-20-2012, 05:33 PM
RE: RH Testing Thick Slabs - CC Solutions - 11-20-2012, 05:35 PM
RE: RH Testing Thick Slabs - CCR - 11-20-2012, 05:45 PM
RE: RH Testing Thick Slabs - CC Solutions - 11-20-2012, 05:49 PM
RE: RH Testing Thick Slabs - CCR - 11-20-2012, 05:54 PM
RE: RH Testing Thick Slabs - eaadams - 11-21-2012, 10:19 AM