The only other thing we know is that Calcium Carbide testing is mainly used to test the moisture content of screeds. Far as I can tell screeds are about the only place you'll find a manufacturer warrantying on a CC test. I had a link but am too lazy to find it right now.Tongue

Whereas...not many flooring/adhesive/VB manufacturers warranty over concrete treated with silicates...

Pat Atherton
Floor Test Australia
www.moisturetesting.com.au

"Democracy ... can only exist until the majority discover they can vote themselves largess out of the public treasury" - Tytler, De Tocqueville, Reagan
Find all posts by this user
Quote this message in a reply
Post Reply 


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious

Messages In This Thread
RE: Calcium Carbide testing and Silicates - Rubensgt40 - 09-18-2012 10:58 PM