Another device to think about when trying to identify tubing, rebar etc. is the Bosch D-tect 150. As long as the slab is no more than 6" thick, it will find almost anything you need in a slab.
Jason |
|||
|
« Next Oldest | Next Newest »
|
![]() |
|||||||
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
|
| Messages In This Thread |
|
Problems in the UK, HELP!!!! - bugs183 - 09-04-2012, 01:42 AM
RE: Problems in the UK, HELP!!!! - Ernesto - 09-04-2012, 07:06 PM
RE: Problems in the UK, HELP!!!! - CC Solutions - 09-05-2012, 06:20 AM
RE: Problems in the UK, HELP!!!! - bugs183 - 09-05-2012, 07:12 AM
RE: Problems in the UK, HELP!!!! - Rubensgt40 - 09-07-2012, 05:36 AM
RE: Problems in the UK, HELP!!!! - bugs183 - 09-07-2012, 12:01 PM
RE: Problems in the UK, HELP!!!! - Rubensgt40 - 09-08-2012, 01:30 AM
RE: Problems in the UK, HELP!!!! - Ernesto - 09-08-2012, 12:31 PM
RE: Problems in the UK, HELP!!!! - eaadams - 09-16-2012, 10:45 PM
RE: Problems in the UK, HELP!!!! - rapidrhrep - 09-17-2012 11:40 AM
RE: Problems in the UK, HELP!!!! - eaadams - 09-18-2012, 09:41 AM
RE: Problems in the UK, HELP!!!! - Rubensgt40 - 09-18-2012, 11:16 PM
RE: Problems in the UK, HELP!!!! - CC Solutions - 09-19-2012, 06:12 AM
RE: Problems in the UK, HELP!!!! - lennyh - 10-02-2012, 04:06 PM
|



Help
Advanced Search



![[-] [-]](images/collapse.gif)