Problems in the UK, HELP!!!!
|
|
09-16-2012, 10:45 PM
Post: #9
|
|||
|
|||
|
RE: Problems in the UK, HELP!!!!
Standard procedure in the USA is to never lay over an active radiant heat system. You run it, turn it off, lay the floor, wait, turn it back on.
Also if you ask Wagner nice enough they may share with you some new 'kit' for such gypcrete. Another thing, here in the USA gypcrete is a brand name, like xerox, you want to be careful about how you use the word. It is 'gypsum based' products. The aforementioned brand, in our experience, always has its own adhesives and most importantly primers to work with their systems. Using those have always been good but all USA flooring people always have instructions to never lay over gypsum based compounds. |
|||
|
« Next Oldest | Next Newest »
|
![]() |
|||||||
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
|
| Messages In This Thread |
|
Problems in the UK, HELP!!!! - bugs183 - 09-04-2012, 01:42 AM
RE: Problems in the UK, HELP!!!! - Ernesto - 09-04-2012, 07:06 PM
RE: Problems in the UK, HELP!!!! - CC Solutions - 09-05-2012, 06:20 AM
RE: Problems in the UK, HELP!!!! - bugs183 - 09-05-2012, 07:12 AM
RE: Problems in the UK, HELP!!!! - Rubensgt40 - 09-07-2012, 05:36 AM
RE: Problems in the UK, HELP!!!! - bugs183 - 09-07-2012, 12:01 PM
RE: Problems in the UK, HELP!!!! - Rubensgt40 - 09-08-2012, 01:30 AM
RE: Problems in the UK, HELP!!!! - Ernesto - 09-08-2012, 12:31 PM
RE: Problems in the UK, HELP!!!! - eaadams - 09-16-2012 10:45 PM
RE: Problems in the UK, HELP!!!! - rapidrhrep - 09-17-2012, 11:40 AM
RE: Problems in the UK, HELP!!!! - eaadams - 09-18-2012, 09:41 AM
RE: Problems in the UK, HELP!!!! - Rubensgt40 - 09-18-2012, 11:16 PM
RE: Problems in the UK, HELP!!!! - CC Solutions - 09-19-2012, 06:12 AM
RE: Problems in the UK, HELP!!!! - lennyh - 10-02-2012, 04:06 PM
|