We're almost at 3lbs MVER, so what if the rH is over 90% ?
08-17-2012, 07:50 AM
Post: #25
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ?
(08-17-2012 07:16 AM)Ernesto Wrote:  To hit that mark would be very rare out here in the Southwest. Besides that, there's other issues with testing before the HVAC is up and running. Think about it.

And I don't think that they meant to say if the site is in the zone of one or two days. This should be corrected immediately.

The ASTM says 48hrs. It's really not rocket science,but people still mess it up.

JD Grafton