Testing Cost
07-26-2012, 09:48 AM (This post was last modified: 07-26-2012 09:49 AM by CC Solutions.)
Post: #15
RE: Testing Cost
Actually you need that 'r' in there or it relates to mental issues, which may not be completely improper when it comes to concrete drying...

A psychrometric chart displays the relationship between air, temp and moisture. Let's see if I can post one here....

Now using that chart it is quite easy to see your concrete is too wet.... Tongue

Or too dry.... Or maybe it's too gray or hard..... Big Grin

The chart looks confusing but really it is quite simple to use. Wink


Attached File(s)
.gif  psychrometric_chart.gif (Size: 74.57 KB / Downloads: 9)

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com
Find all posts by this user
Quote this message in a reply
Post Reply 


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious

Messages In This Thread
Testing Cost - eaadams - 06-06-2012, 07:25 PM
RE: Testing Cost - Ernesto - 06-07-2012, 05:59 PM
RE: Testing Cost - CCR - 06-10-2012, 04:21 AM
RE: Testing Cost - CC Solutions - 06-12-2012, 10:39 AM
RE: Testing Cost - CCR - 06-13-2012, 05:14 PM
RE: Testing Cost - CC Solutions - 06-13-2012, 06:46 PM
RE: Testing Cost - eaadams - 06-14-2012, 10:19 AM
RE: Testing Cost - CC Solutions - 06-14-2012, 10:45 AM
RE: Testing Cost - CCR - 06-14-2012, 05:49 PM
RE: Testing Cost - CC Solutions - 06-14-2012, 07:37 PM
RE: Testing Cost - CCR - 06-15-2012, 05:48 AM
RE: Testing Cost - CCR - 07-26-2012, 08:36 AM
RE: Testing Cost - CC Solutions - 07-26-2012, 08:49 AM
RE: Testing Cost - CCR - 07-26-2012, 08:53 AM
RE: Testing Cost - CC Solutions - 07-26-2012 09:48 AM
RE: Testing Cost - CCR - 07-26-2012, 10:16 AM
RE: Testing Cost - CC Solutions - 07-26-2012, 10:54 AM
RE: Testing Cost - CCR - 07-26-2012, 12:57 PM
RE: Testing Cost - CC Solutions - 07-26-2012, 02:36 PM
RE: Testing Cost - rapidrhrep - 07-27-2012, 08:07 AM
RE: Testing Cost - CCR - 07-27-2012, 12:36 PM
RE: Testing Cost - CC Solutions - 07-30-2012, 04:39 PM
RE: Testing Cost - Ernesto - 07-30-2012, 07:01 PM