(07-24-2012 05:46 PM)CC Solutions Wrote: I never contradict myself. Ever. Then how can you claim CaCL if performed properly is not a valid test? Oh, gotcha. Stephen Perrera dba Top Floor Installation Co. http://www.tucsonazflooring.com http://www.floorsavior.com |
|||
|