Tech data sheets have been updated for Koster and Ardex MC and as you noted, both state 7 day waiting period. However the original MC formula touted it would drop MVER levels from 20lbs to 3 lbs. So, if freshly placed concrete is 28 lbs or so, a drop of 8lbs would make sense (perhaps after 7 days). The variable of course, is still curing and drying conditions. Regardless, noboby claims their products can be installed on fresh concrete. That was just a wrong thing to even consider!
JK Nixon Concrete Restoration Services, LLC Pittsburgh, PA http://www.rhtester.com |
|||
|
« Next Oldest | Next Newest »
|
![]() |
|||||||
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
|
| Messages In This Thread |
|
Mopped the Floor - eaadams - 06-25-2012, 01:44 PM
RE: Mopped the Floor - CC Solutions - 06-25-2012, 02:48 PM
RE: Mopped the Floor - eaadams - 06-28-2012, 04:47 PM
RE: Mopped the Floor - CCR - 07-02-2012, 10:57 AM
RE: Mopped the Floor - rapidrhrep - 07-02-2012, 12:35 PM
RE: Mopped the Floor - CC Solutions - 07-02-2012, 12:47 PM
RE: Mopped the Floor - eaadams - 07-09-2012, 01:30 PM
RE: Mopped the Floor - CCR - 07-10-2012, 11:47 AM
RE: Mopped the Floor - CC Solutions - 07-12-2012, 06:21 AM
RE: Mopped the Floor - eaadams - 07-12-2012, 01:09 PM
RE: Mopped the Floor - CC Solutions - 07-12-2012, 01:35 PM
RE: Mopped the Floor - eaadams - 07-18-2012, 11:15 AM
RE: Mopped the Floor - CC Solutions - 07-19-2012, 07:42 PM
RE: Mopped the Floor - CCR - 07-20-2012, 05:48 AM
RE: Mopped the Floor - CC Solutions - 07-20-2012, 06:17 AM
RE: Mopped the Floor - CCR - 07-20-2012, 06:42 AM
RE: Mopped the Floor - CC Solutions - 07-20-2012, 07:01 AM
RE: Mopped the Floor - CCR - 07-20-2012 07:41 AM
RE: Mopped the Floor - CC Solutions - 07-20-2012, 08:03 AM
RE: Mopped the Floor - CCR - 07-20-2012, 08:21 AM
RE: Mopped the Floor - CC Solutions - 07-20-2012, 08:51 AM
RE: Mopped the Floor - rapidrhrep - 07-20-2012, 11:24 AM
RE: Mopped the Floor - CC Solutions - 07-20-2012, 11:53 AM
|



Help
Advanced Search




![[-] [-]](images/collapse.gif)