RH & CC Testing
|
|
07-17-2012, 12:10 PM
Post: #9
|
|||
|
|||
|
RE: RH & CC Testing
I agree, CCR...I wish that all my projects required the testing to be done by an independent, certified agency.
Not only is it beneficial to owners and clients, but to us as contractors as well. I would much rather not be in the position of monitoring the RH of a slab which is waiting for flooring installation, and having the GC question my every move, asserting that my testing MUST be faulty (because the 5" slab that he poured 6 weeks ago is testing in the high 90% and not moving down by leaps and bounds every day **eyeroll**). Even when you educate them, when they are being ridden by (an unrealistic) schedule, they seem to not get it. I believe if the testing was done independently, they would have a harder time pressuring us to install the flooring before the concrete is ready. Erica Project Manager |
|||
|
« Next Oldest | Next Newest »
|
![]() |
|||||||
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
|
| Messages In This Thread |
|
RH & CC Testing - CCR - 07-10-2012, 10:35 AM
RE: RH & CC Testing - CC Solutions - 07-12-2012, 06:37 AM
RE: RH & CC Testing - CCR - 07-12-2012, 07:25 AM
RE: RH & CC Testing - eaadams - 07-12-2012, 01:31 PM
RE: RH & CC Testing - CCR - 07-12-2012, 01:38 PM
RE: RH & CC Testing - CC Solutions - 07-12-2012, 01:48 PM
RE: RH & CC Testing - JLG - 07-17-2012, 11:13 AM
RE: RH & CC Testing - CCR - 07-17-2012, 11:37 AM
RE: RH & CC Testing - Erica - 07-17-2012 12:10 PM
RE: RH & CC Testing - CCR - 07-17-2012, 12:27 PM
RE: RH & CC Testing - eaadams - 07-18-2012, 11:19 AM
RE: RH & CC Testing - CCR - 07-18-2012, 11:32 AM
RE: RH & CC Testing - CC Solutions - 07-19-2012, 07:49 PM
RE: RH & CC Testing - CCR - 07-22-2012, 04:55 AM
RE: RH & CC Testing - CC Solutions - 07-22-2012, 09:09 AM
RE: RH & CC Testing - CCR - 07-22-2012, 03:05 PM
RE: RH & CC Testing - Rubensgt40 - 07-22-2012, 07:19 PM
RE: RH & CC Testing - CC Solutions - 07-22-2012, 07:33 PM
RE: RH & CC Testing - CCR - 07-24-2012, 04:07 PM
RE: RH & CC Testing - Rubensgt40 - 07-24-2012, 05:35 PM
RE: RH & CC Testing - CC Solutions - 07-24-2012, 05:49 PM
RE: RH & CC Testing - CCR - 07-25-2012, 03:49 AM
RE: RH & CC Testing - Rubensgt40 - 07-25-2012, 09:46 PM
RE: RH & CC Testing - CC Solutions - 07-26-2012, 06:19 AM
|



Help