RE: RH Testing For Parking Garages
Appreciate your input
It appears all their coating systems call for CaCl testing. I can see it now...prep the test area, etc. per ASTM, place the kits and come to find a virtual rain forest inside the plastic cover and pellets solidified into a slimy, solid mass.
JK Nixon Concrete Restoration Services, LLC Pittsburgh, PA http://www.rhtester.com |
|||
|
« Next Oldest | Next Newest »
|
![]() |
|||||||
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
|
| Messages In This Thread |
|
RH Testing For Parking Garages - CCR - 07-12-2012, 07:56 AM
RE: RH Testing For Parking Garages - CC Solutions - 07-12-2012, 08:12 AM
RE: RH Testing For Parking Garages - CCR - 07-12-2012, 08:48 AM
RE: RH Testing For Parking Garages - CC Solutions - 07-12-2012, 09:00 AM
RE: RH Testing For Parking Garages - CCR - 07-12-2012 09:14 AM
RE: RH Testing For Parking Garages - eaadams - 07-12-2012, 01:22 PM
RE: RH Testing For Parking Garages - CCR - 07-12-2012, 01:44 PM
|



Help
Advanced Search

It appears all their coating systems call for CaCl testing. I can see it now...prep the test area, etc. per ASTM, place the kits and come to find a virtual rain forest inside the plastic cover and pellets solidified into a slimy, solid mass.



![[-] [-]](images/collapse.gif)