RH Testing For Parking Garages
|
|
07-12-2012, 08:48 AM
Post: #3
|
|||
|
|||
|
RE: RH Testing For Parking Garages
Well, it's Pittsburgh, what can I say except temp at testing time was my first concern too. But this is no place to do Calcium Chloride tests. I would anticipate performing tests in the late spring thru early fall about the same time and ambient conditions the coating systems are to be applied. So technically, they would be conducted in conditions the manufacturer would recognize as acclimated (for application anyway). Other than that, I can think of nothing else to be concerned with off the top of my head.
I'm writing "blindly" right now because I have not read the manufacturer's literature yet. That's next Always something new to consider, right? JK Nixon Concrete Restoration Services, LLC Pittsburgh, PA http://www.rhtester.com |
|||
|
« Next Oldest | Next Newest »
|
![]() |
|||||||
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
|
| Messages In This Thread |
|
RH Testing For Parking Garages - CCR - 07-12-2012, 07:56 AM
RE: RH Testing For Parking Garages - CC Solutions - 07-12-2012, 08:12 AM
RE: RH Testing For Parking Garages - CCR - 07-12-2012 08:48 AM
RE: RH Testing For Parking Garages - CC Solutions - 07-12-2012, 09:00 AM
RE: RH Testing For Parking Garages - CCR - 07-12-2012, 09:14 AM
RE: RH Testing For Parking Garages - eaadams - 07-12-2012, 01:22 PM
RE: RH Testing For Parking Garages - CCR - 07-12-2012, 01:44 PM
|