Ardex V1200
|
|
07-12-2012, 07:49 AM
Post: #19
|
|||
|
|||
|
RE: Ardex V1200
I had the opportunity to test a self-leveler very similar to V1200 from a newer manufacturer recently. While it was "OK", it didn't spread and finish like Ardex...simple as that. Ya get what ya pay for every time no matter what.
JK Nixon Concrete Restoration Services, LLC Pittsburgh, PA http://www.rhtester.com |
|||
|
« Next Oldest | Next Newest »
|
![]() |
|||||||
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
|
| Messages In This Thread |
|
Ardex V1200 - CC Solutions - 03-27-2012, 09:57 AM
RE: Ardex V1200 - eaadams - 03-27-2012, 10:03 AM
RE: Ardex V1200 - CC Solutions - 03-27-2012, 10:36 AM
RE: Ardex V1200 - eaadams - 04-25-2012, 02:01 PM
RE: Ardex V1200 - CC Solutions - 04-25-2012, 04:06 PM
RE: Ardex V1200 - CCR - 04-26-2012, 04:36 AM
RE: Ardex V1200 - CC Solutions - 04-26-2012, 06:11 AM
RE: Ardex V1200 - CCR - 04-26-2012, 07:11 AM
RE: Ardex V1200 - CC Solutions - 04-26-2012, 07:18 AM
RE: Ardex V1200 - CCR - 04-26-2012, 07:33 AM
RE: Ardex V1200 - CC Solutions - 04-26-2012, 07:16 PM
RE: Ardex V1200 - eaadams - 04-26-2012, 08:36 PM
RE: Ardex V1200 - CC Solutions - 04-27-2012, 06:06 AM
RE: Ardex V1200 - eaadams - 05-07-2012, 09:45 AM
RE: Ardex V1200 - CC Solutions - 05-07-2012, 12:27 PM
RE: Ardex V1200 - eaadams - 07-10-2012, 10:28 AM
RE: Ardex V1200 - CCR - 07-10-2012, 11:40 AM
RE: Ardex V1200 - CC Solutions - 07-12-2012, 06:19 AM
RE: Ardex V1200 - CCR - 07-12-2012 07:49 AM
RE: Ardex V1200 - CC Solutions - 07-12-2012, 08:10 AM
RE: Ardex V1200 - eaadams - 07-12-2012, 12:56 PM
RE: Ardex V1200 - CC Solutions - 07-12-2012, 01:33 PM
RE: Ardex V1200 - eaadams - 07-12-2012, 01:42 PM
RE: Ardex V1200 - CC Solutions - 07-12-2012, 01:50 PM
RE: Ardex V1200 - CCR - 07-12-2012, 02:46 PM
RE: Ardex V1200 - CC Solutions - 07-12-2012, 04:25 PM
|



Help
Advanced Search



![[-] [-]](images/collapse.gif)