Can tape over the probe cause erroneous readings?
|
|
07-03-2012, 01:20 PM
Post: #11
|
|||
|
|||
RE: Can tape over the probe cause erroneous readings?
(07-03-2012 12:44 PM)rthompson Wrote: No, It doesn't matter if you put tape over the hole or not I agree the initial reading is not affected by tape, but what about putting a vapor retarding duct tape over the probe for four months as you track RH? And you know some guys put a nice big area of tape down, 3 strips wide and 3 strips across, so basically a 6" square of vapor retarder over the probe. JD Grafton Concrete Answers for Flooring Problems JGrafton@ccsolves.com |
|||
|