Thanks Jason.
Then we have to consider how much water went in the hole (if any) and how does that affect the readings we are seeing now. The concrete could absorb some water and the hole could be dry, but the concrete may now be saturated and readings would be higher than normal. My thoughts are if there is any suspicion at all and your credibility rides on proper readings, install new probes. Then again if maybe one or two probes may or may not have seen water, just correlate those readings with others and see where they fall. If they all jive, the probes probably didn't get wet. If those probes are reading high, don't publish the results. JD Grafton Concrete Answers for Flooring Problems JGrafton@ccsolves.com |
|||
|
« Next Oldest | Next Newest »
|
![]() |
|||||||
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
|
| Messages In This Thread |
|
Mopped the Floor - eaadams - 06-25-2012, 01:44 PM
RE: Mopped the Floor - CC Solutions - 06-25-2012, 02:48 PM
RE: Mopped the Floor - eaadams - 06-28-2012, 04:47 PM
RE: Mopped the Floor - CCR - 07-02-2012, 10:57 AM
RE: Mopped the Floor - rapidrhrep - 07-02-2012, 12:35 PM
RE: Mopped the Floor - CC Solutions - 07-02-2012 12:47 PM
RE: Mopped the Floor - eaadams - 07-09-2012, 01:30 PM
RE: Mopped the Floor - CCR - 07-10-2012, 11:47 AM
RE: Mopped the Floor - CC Solutions - 07-12-2012, 06:21 AM
RE: Mopped the Floor - eaadams - 07-12-2012, 01:09 PM
RE: Mopped the Floor - CC Solutions - 07-12-2012, 01:35 PM
RE: Mopped the Floor - eaadams - 07-18-2012, 11:15 AM
RE: Mopped the Floor - CC Solutions - 07-19-2012, 07:42 PM
RE: Mopped the Floor - CCR - 07-20-2012, 05:48 AM
RE: Mopped the Floor - CC Solutions - 07-20-2012, 06:17 AM
RE: Mopped the Floor - CCR - 07-20-2012, 06:42 AM
RE: Mopped the Floor - CC Solutions - 07-20-2012, 07:01 AM
RE: Mopped the Floor - CCR - 07-20-2012, 07:41 AM
RE: Mopped the Floor - CC Solutions - 07-20-2012, 08:03 AM
RE: Mopped the Floor - CCR - 07-20-2012, 08:21 AM
RE: Mopped the Floor - CC Solutions - 07-20-2012, 08:51 AM
RE: Mopped the Floor - rapidrhrep - 07-20-2012, 11:24 AM
RE: Mopped the Floor - CC Solutions - 07-20-2012, 11:53 AM
|



Help
Advanced Search



![[-] [-]](images/collapse.gif)