Can tape over the probe cause erroneous readings?
06-25-2012, 11:38 PM (This post was last modified: 06-25-2012 11:39 PM by eaadams.)
Post: #5
RE: Can tape over the probe cause erroneous readings?
Well I have two testers doing this now. I have not seen a difference. I have seen one set of tests start around 99 and they got down to the low 90's

edit ....

over three months
99 to 86
94 to dead probe
90 to 80
99 to 90
96 to 81
99 to 85
99 to 91
99 to 85