06-19-2012, 11:29 AM
Post: #1
|
|||
|
|||
|
Wagner Article Vapor Retarders
http://www.wagnermeters.com/external-inf...Newsletter
Check your language. ACI has specific guidelines for the words "Vapor Retarders". I think you are talking more "Vapor Barriers" It is all about the perms and under the slab you want a Barrier at or less than 0.01 perms, stego or equal |
|||
|