Hi everyone... I'm new here and love this thread. There is no question that there is a lot of confusion over the evaluation of moisture in concrete slabs. I especially love the people that put their electronic meter on a slab - observe the red light flashing and the beeping sound coming from this device - and then pronounce the slab to be "too wet". Sheesh!
Meters are Guides... NOT Gods! So - I have a question for CC... Based on your message dated 03/18, you have a somewhat similar ERH reading in the slab - yet the MVER are on two ends of the 'acceptability spectrum'. When using the Rapid RH device, what is considered to be 'acceptable'? Thanks guys! Ken Larsen |
|||
|