Substrate Odor
|
|
05-23-2012, 07:38 AM
Post: #13
|
|||
|
|||
|
RE: Substrate Odor
If there is standing water under the slab, mitigating one part won't increase the amount of water under another part. That would be saying the portion you have mitigated was substantially drying the slab in one area and you have now plugged the leak in the dam. That just doesn't happen.
JD Grafton Concrete Answers for Flooring Problems JGrafton@ccsolves.com |
|||
|
« Next Oldest | Next Newest »
|
![]() |
|||||||
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
|
| Messages In This Thread |
|
Substrate Odor - CCR - 05-19-2012, 06:06 AM
RE: Substrate Odor - CC Solutions - 05-20-2012, 09:15 AM
RE: Substrate Odor - CCR - 05-20-2012, 02:07 PM
RE: Substrate Odor - CC Solutions - 05-20-2012, 10:18 PM
RE: Substrate Odor - CCR - 05-21-2012, 03:34 AM
RE: Substrate Odor - CC Solutions - 05-21-2012, 06:45 AM
RE: Substrate Odor - Matt S - 05-22-2012, 06:19 PM
RE: Substrate Odor - CC Solutions - 05-22-2012, 07:07 PM
RE: Substrate Odor - Matt S - 05-22-2012, 07:16 PM
RE: Substrate Odor - CCR - 05-23-2012, 06:02 AM
RE: Substrate Odor - CC Solutions - 05-23-2012, 06:16 AM
RE: Substrate Odor - Matt S - 05-23-2012, 06:58 AM
RE: Substrate Odor - CC Solutions - 05-23-2012 07:38 AM
RE: Substrate Odor - CCR - 05-23-2012, 07:46 AM
RE: Substrate Odor - Matt S - 05-23-2012, 09:51 AM
RE: Substrate Odor - eaadams - 05-24-2012, 12:58 PM
RE: Substrate Odor - CCR - 05-24-2012, 04:45 PM
RE: Substrate Odor - CC Solutions - 05-27-2012, 09:54 PM
RE: Substrate Odor - CCR - 06-15-2012, 11:02 AM
RE: Substrate Odor - CCR - 07-15-2012, 06:15 AM
RE: Substrate Odor - eaadams - 07-18-2012, 11:09 AM
RE: Substrate Odor - CCR - 07-18-2012, 11:36 AM
|



Help
Advanced Search



![[-] [-]](images/collapse.gif)