Substrate Odor
|
|
05-23-2012, 06:02 AM
Post: #10
|
|||
|
|||
|
RE: Substrate Odor
Compare MVE to a pot of boiling water... steam does not move sideways as it rises out of the pot. Same principal. Moisture vapor emissions move straight up, yet CAN migrate latteraly to some degree. Therefore, I was trained to add a foor or two to the perimeter of any MM system installation similar to mine.
Update: I provided an estimate yesterday to the customer covering the "conservative" fix, vs. installation of a MM system. For about $700 more, they get a warranted fix. I suspect they will go with the system and be done with this problem. JK Nixon Concrete Restoration Services, LLC Pittsburgh, PA http://www.rhtester.com |
|||
|
« Next Oldest | Next Newest »
|
![]() |
|||||||
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
|
| Messages In This Thread |
|
Substrate Odor - CCR - 05-19-2012, 06:06 AM
RE: Substrate Odor - CC Solutions - 05-20-2012, 09:15 AM
RE: Substrate Odor - CCR - 05-20-2012, 02:07 PM
RE: Substrate Odor - CC Solutions - 05-20-2012, 10:18 PM
RE: Substrate Odor - CCR - 05-21-2012, 03:34 AM
RE: Substrate Odor - CC Solutions - 05-21-2012, 06:45 AM
RE: Substrate Odor - Matt S - 05-22-2012, 06:19 PM
RE: Substrate Odor - CC Solutions - 05-22-2012, 07:07 PM
RE: Substrate Odor - Matt S - 05-22-2012, 07:16 PM
RE: Substrate Odor - CCR - 05-23-2012 06:02 AM
RE: Substrate Odor - CC Solutions - 05-23-2012, 06:16 AM
RE: Substrate Odor - Matt S - 05-23-2012, 06:58 AM
RE: Substrate Odor - CC Solutions - 05-23-2012, 07:38 AM
RE: Substrate Odor - CCR - 05-23-2012, 07:46 AM
RE: Substrate Odor - Matt S - 05-23-2012, 09:51 AM
RE: Substrate Odor - eaadams - 05-24-2012, 12:58 PM
RE: Substrate Odor - CCR - 05-24-2012, 04:45 PM
RE: Substrate Odor - CC Solutions - 05-27-2012, 09:54 PM
RE: Substrate Odor - CCR - 06-15-2012, 11:02 AM
RE: Substrate Odor - CCR - 07-15-2012, 06:15 AM
RE: Substrate Odor - eaadams - 07-18-2012, 11:09 AM
RE: Substrate Odor - CCR - 07-18-2012, 11:36 AM
|