Ardex V1200
04-26-2012, 07:16 PM
Post: #11
RE: Ardex V1200
K15 is $31 a bag. V1200 is $20 a bag. The difference is the polymers in the K15 which allow it to dry in 16 hours instead of three days.

So when you say the difference in cost is negligible, I have to question if you are thinking from a buyer's point of view or a seller's??? When a bag only covers 2 or 3 square feet at that thickness you can quickly add $4 to $6 per square foot for the product alone.

Both products can do the same job if you work with their differing qualities.

I have added pea gravel to V1200 before also. And K15.
Suffice it to say that there is a lot more to know about levelers than mix the water, pour it out and get paid on Friday. If it was that easy anyone could do it.

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com
Find all posts by this user
Quote this message in a reply
Post Reply 


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious

Messages In This Thread
Ardex V1200 - CC Solutions - 03-27-2012, 09:57 AM
RE: Ardex V1200 - eaadams - 03-27-2012, 10:03 AM
RE: Ardex V1200 - CC Solutions - 03-27-2012, 10:36 AM
RE: Ardex V1200 - eaadams - 04-25-2012, 02:01 PM
RE: Ardex V1200 - CC Solutions - 04-25-2012, 04:06 PM
RE: Ardex V1200 - CCR - 04-26-2012, 04:36 AM
RE: Ardex V1200 - CC Solutions - 04-26-2012, 06:11 AM
RE: Ardex V1200 - CCR - 04-26-2012, 07:11 AM
RE: Ardex V1200 - CC Solutions - 04-26-2012, 07:18 AM
RE: Ardex V1200 - CCR - 04-26-2012, 07:33 AM
RE: Ardex V1200 - CC Solutions - 04-26-2012 07:16 PM
RE: Ardex V1200 - eaadams - 04-26-2012, 08:36 PM
RE: Ardex V1200 - CC Solutions - 04-27-2012, 06:06 AM
RE: Ardex V1200 - eaadams - 05-07-2012, 09:45 AM
RE: Ardex V1200 - CC Solutions - 05-07-2012, 12:27 PM
RE: Ardex V1200 - eaadams - 07-10-2012, 10:28 AM
RE: Ardex V1200 - CCR - 07-10-2012, 11:40 AM
RE: Ardex V1200 - CC Solutions - 07-12-2012, 06:19 AM
RE: Ardex V1200 - CCR - 07-12-2012, 07:49 AM
RE: Ardex V1200 - CC Solutions - 07-12-2012, 08:10 AM
RE: Ardex V1200 - eaadams - 07-12-2012, 12:56 PM
RE: Ardex V1200 - CC Solutions - 07-12-2012, 01:33 PM
RE: Ardex V1200 - eaadams - 07-12-2012, 01:42 PM
RE: Ardex V1200 - CC Solutions - 07-12-2012, 01:50 PM
RE: Ardex V1200 - CCR - 07-12-2012, 02:46 PM
RE: Ardex V1200 - CC Solutions - 07-12-2012, 04:25 PM