How thick is your floor?
04-11-2012, 06:30 AM
Post: #16
RE: How thick is your floor?
(04-10-2012 08:41 PM)Ernesto Wrote:  Just because you fill the puncture with epoxy; does that unequivocally insure the puncture is sealed? I hardly think so.

Yes that insures the puncture is sealed. This is how we seal cracks, holes and repairs. That epoxy is many times stronger than the concrete, and many times more waterproof. Wink

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com
Find all posts by this user
Quote this message in a reply
Post Reply 


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious

Messages In This Thread
How thick is your floor? - CC Solutions - 03-27-2012, 10:23 AM
RE: How thick is your floor? - eaadams - 03-27-2012, 01:14 PM
RE: How thick is your floor? - Ernesto - 03-27-2012, 08:08 PM
RE: How thick is your floor? - eaadams - 03-31-2012, 08:23 PM
RE: How thick is your floor? - Ernesto - 04-01-2012, 09:14 AM
RE: How thick is your floor? - CCR - 04-02-2012, 09:53 PM
RE: How thick is your floor? - eaadams - 04-03-2012, 09:56 AM
RE: How thick is your floor? - Ernesto - 04-10-2012, 08:02 PM
RE: How thick is your floor? - Ernesto - 04-10-2012, 08:41 PM
RE: How thick is your floor? - CC Solutions - 04-11-2012 06:30 AM
RE: How thick is your floor? - Ernesto - 04-11-2012, 06:57 AM