How thick is your floor?
04-10-2012, 06:14 PM (This post was last modified: 04-10-2012 06:18 PM by Rubensgt40.)
Post: #11
RE: How thick is your floor?
I've noticed this brought up on other threads- how can you be sure you're adhering to the letter of F2170 without knowing the exact slab depth?

I suppose if it went to a claims court you'd argue that the builder's specs were the only credible source.

And... if you drilled a depth test hole, wouldn't that puncture the under-slab retarder?

That StructureScan toy might not be such a bad idea. How expensive can they be? Big Grin

Pat Atherton
Floor Test Australia
www.moisturetesting.com.au

"Democracy ... can only exist until the majority discover they can vote themselves largess out of the public treasury" - Tytler, De Tocqueville, Reagan
Find all posts by this user
Quote this message in a reply
04-10-2012, 07:29 PM
Post: #12
RE: How thick is your floor?
Yes I puncture the vapor retarder when I drill through, then I fill the holes with epoxy. It's the only sure-fire way of determining depth I know of.

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com
Find all posts by this user
Quote this message in a reply
04-10-2012, 08:02 PM
Post: #13
RE: How thick is your floor?
(04-10-2012 07:29 PM)CC Solutions Wrote:  Yes I puncture the vapor retarder when I drill through, then I fill the holes with epoxy. It's the only sure-fire way of determining depth I know of.

You mean besides the scanner.

Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com
Visit this user's website Find all posts by this user
Quote this message in a reply
04-10-2012, 08:16 PM
Post: #14
RE: How thick is your floor?
You have a scanner that can tell me the depth of concrete on a compacted stone base to within 1/2"?

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com
Find all posts by this user
Quote this message in a reply
04-10-2012, 08:41 PM
Post: #15
RE: How thick is your floor?
Just because you fill the puncture with epoxy; does that unequivocally insure the puncture is sealed? I hardly think so.

Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com
Visit this user's website Find all posts by this user
Quote this message in a reply
04-11-2012, 06:30 AM
Post: #16
RE: How thick is your floor?
(04-10-2012 08:41 PM)Ernesto Wrote:  Just because you fill the puncture with epoxy; does that unequivocally insure the puncture is sealed? I hardly think so.

Yes that insures the puncture is sealed. This is how we seal cracks, holes and repairs. That epoxy is many times stronger than the concrete, and many times more waterproof. Wink

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com
Find all posts by this user
Quote this message in a reply
04-11-2012, 06:57 AM
Post: #17
RE: How thick is your floor?
So, your going to drill a test hole at every test site to insure your within 1/2 inch huh?

Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com
Visit this user's website Find all posts by this user
Quote this message in a reply
04-11-2012, 07:36 AM
Post: #18
RE: How thick is your floor?
Not at all. At least not with slab on grade concrete. The testing protocol laid out in 2170 does a good job of exposing abnormalities, and any noted discrepancies can be further investigated by drilling confirming test holes for depth. So what I'm saying is if we install probes near exterior walls, near entrances and sprinkled throughout after that, and we know what the designed depth of the slab should be, a couple of proofing holes is all that would be required for a standard test. If probe readings start coming in all over the charts or if an installer wants to push the limits of a test, we may do more proofing.

Slabs in pans need to either use a floor scan tool or be drilled for depth to locate the flutes.

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com
Find all posts by this user
Quote this message in a reply
Post Reply 


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious