How thick is your floor?
|
|
03-27-2012, 01:14 PM
Post: #2
|
|||
|
|||
|
RE: How thick is your floor?
When you took the 8" thickness core was there a vapor retarder 4" down?
If there is a grade beam I guess there wouldn't be a vapor retarder but if you get the cores polished would a break be evident. Interesting.... going to follow this thread. When you say failing what do you mean? the new high ph and high moisture installation systems fail differently than the old school 75% type failures. |
|||
|