improper probe depth
|
|
02-23-2012, 01:00 PM
Post: #1
|
|||
|
|||
|
improper probe depth
After 4 years of drilling and reading Rh levels once or twice a year for our company, I just learned yesterday, because of concerns on my part for consistently getting high readings, and from viewing this website, of the 40/20 depth requirement for proper readings. Yeah WOW! - That's what I said.
My training consisted of verbal instruction from a co-worker who had performed tests initially, and is no longer with the company, to reading the directions that came with the early readers. "Drill your holes 1 3/4 - 2" deep", he said. From what I have learned in the last two days of research, on my own time and of my own initiative, is that I have been doing the tests correctly in every step, except for this one. Now my superiors at my company are blaming me for not doing the tests correctly. Even though I was never given adequate instruction, I feel my job is in jeopardy. I do tests when asked to (infrequently), and I'm an installer (35 years experience, 17yrs. w/ company) primarily. This lapse has cost us a lot of money, not to mention unreliable results. Since I am not certified, and our company, not wanting to be held legally responsible for giving a go ahead for installation after high readings, another testing company is being brought in to verify our results. More time and money spent! I want to be proficient at testing, and feel I am close, thanks to the information I have gained here. I will plead my case to my superiors for more education/knowledge/certification and see what happens. You guys really are Concrete Gurus! Now to my question: having drilled holes 2" deep in a slab that is 3" thick, poured over a corrugated pan appox. 1/8" thick (according to some field measurements taken), what would the correct depth of holes be for the probes? .6" or 1.2" 20% or 40%? Also, if drilling .6", won't the probes stick out 1" above the slab? Is this normal, and how do you prevent them from damage from lifts, bakers, etc.? I need to know where I made my mistake,for my own piece of mind, so hopefully, this will not occur ever again. |
|||
|
« Next Oldest | Next Newest »
|
![]() |
|||||||
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
|
| Messages In This Thread |
|
improper probe depth - Rrozema - 02-23-2012 01:00 PM
RE: improper probe depth - rapidrhrep - 02-23-2012, 01:51 PM
RE: improper probe depth - Rrozema - 02-23-2012, 02:22 PM
RE: improper probe depth - Rrozema - 02-28-2012, 08:44 AM
RE: improper probe depth - rapidrhrep - 03-01-2012, 07:43 AM
RE: improper probe depth - CC Solutions - 03-01-2012, 12:47 PM
RE: improper probe depth - Rubensgt40 - 03-04-2012, 03:56 PM
RE: improper probe depth - CCR - 03-09-2012, 06:14 AM
RE: improper probe depth - GP-CA - 03-23-2012, 02:24 PM
RE: improper probe depth - Ernesto - 03-23-2012, 07:51 PM
RE: improper probe depth - CC Solutions - 03-24-2012, 06:12 AM
|



Help
Advanced Search



![[-] [-]](images/collapse.gif)