I think the economy is improving
01-17-2012, 07:38 AM
Post: #13
RE: I think the economy is improving
(01-16-2012 08:39 AM)Ernesto Wrote:  Not sure what was so funny about my post. Making cementacious products is not rocket science.

Making cementitious products IS like rocket science! Talk to Tim Murphy at Mineralogy for about 30 minutes..... Or ask Wiss Janney Elstner about the science of cementitious underlayments and overlays.

Did you know that only two people know the recipe for K15? Do you know how many people have tried to copy K15 and Feather Finish over the last 20-30 years?

It's not rocket science, but it's as close as you can get. Big Grin

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com
Find all posts by this user
Quote this message in a reply
Post Reply 


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious

Messages In This Thread
I think the economy is improving - eaadams - 01-14-2012, 02:18 AM
RE: I think the economy is improving - CCR - 01-15-2012, 02:02 PM
RE: I think the economy is improving - CC Solutions - 01-17-2012 07:38 AM
RE: I think the economy is improving - CCR - 03-27-2012, 06:01 PM
RE: I think the economy is improving - CCR - 03-27-2012, 09:48 PM