Adhesives and Moisture
02-17-2010, 10:12 PM
Post: #6
RE: Adhesives and Moisture
Ha ha ha .... Now you know what it's like to be old like me!

Say I just got a job on a slab with no vapor retarder and on a sand bed. It has a long history of water problems, but over the last 6 months has been gutted and is being added to and remodeled. The old slab right now is reading 3 - 4 lbs MVER and I was asked to mitigate for moisture. The principals know as soon as they put a floor back on the concrete they will have problems again...

Nice job too.... about 24,000 sf. Big Grin

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com
Find all posts by this user
Quote this message in a reply
Post Reply 


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious

Messages In This Thread
Adhesives and Moisture - Ernesto - 02-03-2010, 01:41 PM
RE: Adhesives and Moisture - CC Solutions - 02-03-2010, 03:53 PM
RE: Adhesives and Moisture - Ernesto - 02-05-2010, 08:12 AM
RE: Adhesives and Moisture - CC Solutions - 02-05-2010, 11:56 AM
RE: Adhesives and Moisture - Ernesto - 02-17-2010, 03:32 PM
RE: Adhesives and Moisture - CC Solutions - 02-17-2010 10:12 PM
RE: Adhesives and Moisture - Ernesto - 02-18-2010, 09:04 AM
RE: Adhesives and Moisture - CC Solutions - 02-18-2010, 09:34 AM
RE: Adhesives and Moisture - Ernesto - 02-18-2010, 03:19 PM
RE: Adhesives and Moisture - CC Solutions - 02-19-2010, 07:13 AM
RE: Adhesives and Moisture - Ernesto - 02-19-2010, 08:34 AM
RE: Adhesives and Moisture - CC Solutions - 02-19-2010, 11:07 AM
RE: Adhesives and Moisture - Ernesto - 02-19-2010, 05:31 PM
RE: Adhesives and Moisture - Ernesto - 03-08-2010, 03:11 PM
RE: Adhesives and Moisture - CC Solutions - 03-09-2010, 06:48 PM
RE: Adhesives and Moisture - Ernesto - 03-10-2010, 03:06 PM
RE: Adhesives and Moisture - CC Solutions - 03-18-2010, 06:31 PM
RE: Adhesives and Moisture - Ernesto - 03-19-2010, 06:01 PM
RE: Adhesives and Moisture - tbrown - 04-08-2010, 10:24 AM
RE: Adhesives and Moisture - CC Solutions - 04-08-2010, 08:10 PM
RE: Adhesives and Moisture - CC Solutions - 04-30-2010, 09:03 AM
RE: Adhesives and Moisture - CC Solutions - 05-01-2010, 09:40 AM
RE: Adhesives and Moisture - CC Solutions - 05-02-2010, 08:18 AM