02-03-2010, 01:41 PM
Post: #1
|
|||
|
|||
|
Adhesives and Moisture
Food for thought:
A little tidbit I found in some lit: 302.2R-18 ACI COMMITTEE REPORT "shown that the adhesive strength decreases with an increase in the concrete’s MVER. When these tests were conducted, however, there were no criteria for acceptable bond strength, and scatter in the test results did not indicate a clear dividing line between acceptable and nonacceptable adhesive bond strength. A report on recent testing that attempted to correlate moisture in the concrete with floor covering performance concluded that: “The evidence presented suggests that there is no relationship between the relative humidity of a concrete base or screed and adhesion of resilient floor coverings” (The Concrete Society 2004). While moisture criteria are often used, the relationship between these criteria and floor covering performance is not well understood." |
|||
|