Uniform seams, opening everywhere, cept in the older section which the owner has not replaced yet. Older section exhibits no problems. No cracking or discolorization anywhere old or new.
Plasticizer migration to what, the new adhesive? The seams are not even curling. Maybe it is just bad vinyl. I was only hired to perform the moisture testing. Stephen Perrera dba Top Floor Installation Co. http://www.tucsonazflooring.com http://www.floorsavior.com |
|||
|
« Next Oldest | Next Newest »
|
![]() |
|||||||
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
|
| Messages In This Thread |
|
Vet Clinic - Ernesto - 12-04-2011, 09:58 AM
RE: Vet Clinic - CC Solutions - 12-05-2011, 06:33 PM
RE: Vet Clinic - eaadams - 12-05-2011, 06:37 PM
RE: Vet Clinic - Ernesto - 12-05-2011, 07:11 PM
RE: Vet Clinic - eaadams - 12-06-2011, 10:33 AM
RE: Vet Clinic - Ernesto - 12-06-2011, 10:42 AM
RE: Vet Clinic - eaadams - 12-06-2011, 01:38 PM
RE: Vet Clinic - Ernesto - 12-06-2011 02:06 PM
RE: Vet Clinic - eaadams - 12-06-2011, 02:48 PM
RE: Vet Clinic - Ernesto - 12-07-2011, 11:59 AM
RE: Vet Clinic - CC Solutions - 12-07-2011, 12:07 PM
RE: Vet Clinic - Ernesto - 12-07-2011, 12:53 PM
RE: Vet Clinic - CC Solutions - 12-07-2011, 01:17 PM
RE: Vet Clinic - eaadams - 12-07-2011, 02:26 PM
RE: Vet Clinic - CC Solutions - 12-07-2011, 02:45 PM
RE: Vet Clinic - Ernesto - 12-07-2011, 04:06 PM
RE: Vet Clinic - CC Solutions - 12-07-2011, 04:36 PM
RE: Vet Clinic - Ernesto - 12-07-2011, 07:58 PM
RE: Vet Clinic - CC Solutions - 12-08-2011, 12:02 AM
RE: Vet Clinic - eaadams - 12-23-2011, 12:15 PM
RE: Vet Clinic - Ernesto - 12-23-2011, 10:31 PM
|



Help
Advanced Search



![[-] [-]](images/collapse.gif)