Vet Clinic
|
|
12-05-2011, 07:11 PM
(This post was last modified: 12-05-2011 07:12 PM by Ernesto.)
Post: #4
|
|||
|
|||
|
RE: Vet Clinic
I guess the super duper adhesive is working. Otherwise it should be blowing off the floor. I got new readings, 2 out of 3 were "Hi", the other was 97% rh. Me thinks they brought it in hot and installed with HVAC going. Still the vet clinic is a crappy layout, coved, so it was not a blow and go install, yes heat welded seams.
Stephen Perrera dba Top Floor Installation Co. http://www.tucsonazflooring.com http://www.floorsavior.com |
|||
|
« Next Oldest | Next Newest »
|
![]() |
|||||||
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
|
| Messages In This Thread |
|
Vet Clinic - Ernesto - 12-04-2011, 09:58 AM
RE: Vet Clinic - CC Solutions - 12-05-2011, 06:33 PM
RE: Vet Clinic - eaadams - 12-05-2011, 06:37 PM
RE: Vet Clinic - Ernesto - 12-05-2011 07:11 PM
RE: Vet Clinic - eaadams - 12-06-2011, 10:33 AM
RE: Vet Clinic - Ernesto - 12-06-2011, 10:42 AM
RE: Vet Clinic - eaadams - 12-06-2011, 01:38 PM
RE: Vet Clinic - Ernesto - 12-06-2011, 02:06 PM
RE: Vet Clinic - eaadams - 12-06-2011, 02:48 PM
RE: Vet Clinic - Ernesto - 12-07-2011, 11:59 AM
RE: Vet Clinic - CC Solutions - 12-07-2011, 12:07 PM
RE: Vet Clinic - Ernesto - 12-07-2011, 12:53 PM
RE: Vet Clinic - CC Solutions - 12-07-2011, 01:17 PM
RE: Vet Clinic - eaadams - 12-07-2011, 02:26 PM
RE: Vet Clinic - CC Solutions - 12-07-2011, 02:45 PM
RE: Vet Clinic - Ernesto - 12-07-2011, 04:06 PM
RE: Vet Clinic - CC Solutions - 12-07-2011, 04:36 PM
RE: Vet Clinic - Ernesto - 12-07-2011, 07:58 PM
RE: Vet Clinic - CC Solutions - 12-08-2011, 12:02 AM
RE: Vet Clinic - eaadams - 12-23-2011, 12:15 PM
RE: Vet Clinic - Ernesto - 12-23-2011, 10:31 PM
|



Help
Advanced Search



![[-] [-]](images/collapse.gif)