Pm me some pics. All cheap vinyl shrink. Seams should not open up if properly heatwelded. Or were they chemical welded?
If the the vinyl shrinks like that it could be an instalation problem. When vinyl has a moisture problem it should bubble and not stick. If seams open it can be a sign of moisture problems coming but usually it is poor woorksmanship. |
|||
|
« Next Oldest | Next Newest »
|
![]() |
|||||||
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
|
| Messages In This Thread |
|
Vet Clinic - Ernesto - 12-04-2011, 09:58 AM
RE: Vet Clinic - CC Solutions - 12-05-2011, 06:33 PM
RE: Vet Clinic - eaadams - 12-05-2011 06:37 PM
RE: Vet Clinic - Ernesto - 12-05-2011, 07:11 PM
RE: Vet Clinic - eaadams - 12-06-2011, 10:33 AM
RE: Vet Clinic - Ernesto - 12-06-2011, 10:42 AM
RE: Vet Clinic - eaadams - 12-06-2011, 01:38 PM
RE: Vet Clinic - Ernesto - 12-06-2011, 02:06 PM
RE: Vet Clinic - eaadams - 12-06-2011, 02:48 PM
RE: Vet Clinic - Ernesto - 12-07-2011, 11:59 AM
RE: Vet Clinic - CC Solutions - 12-07-2011, 12:07 PM
RE: Vet Clinic - Ernesto - 12-07-2011, 12:53 PM
RE: Vet Clinic - CC Solutions - 12-07-2011, 01:17 PM
RE: Vet Clinic - eaadams - 12-07-2011, 02:26 PM
RE: Vet Clinic - CC Solutions - 12-07-2011, 02:45 PM
RE: Vet Clinic - Ernesto - 12-07-2011, 04:06 PM
RE: Vet Clinic - CC Solutions - 12-07-2011, 04:36 PM
RE: Vet Clinic - Ernesto - 12-07-2011, 07:58 PM
RE: Vet Clinic - CC Solutions - 12-08-2011, 12:02 AM
RE: Vet Clinic - eaadams - 12-23-2011, 12:15 PM
RE: Vet Clinic - Ernesto - 12-23-2011, 10:31 PM
|



Help
Advanced Search


![[-] [-]](images/collapse.gif)