CaCl and RH correlation?
01-27-2010, 10:35 AM
Post: #15
RE: CaCl and RH correlation?
With a good vapor barrier under the slab this is a non-issue. Without a good vapor barrier under the slab there will ALWAYS be moisture going into the slab.

(guess I don't need to read page 22 Tongue )

I still haven't found the book. Sorry.....

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com
Find all posts by this user
Quote this message in a reply
Post Reply 


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious

Messages In This Thread
CaCl and RH correlation? - Bryan F - 09-12-2008, 05:40 PM
RE: CaCl and RH correlation? - rthompson - 09-15-2008, 04:24 PM
RE: CaCl and RH correlation? - Bryan F - 09-26-2008, 09:48 AM
RE: CaCl and RH correlation? - CMoore - 10-02-2008, 01:43 PM
RE: CaCl and RH correlation? - rthompson - 10-21-2008, 11:56 AM
RE: CaCl and RH correlation? - Ernesto - 01-12-2010, 09:54 AM
RE: CaCl and RH correlation? - Ernesto - 01-13-2010, 03:26 PM
RE: CaCl and RH correlation? - Ernesto - 01-16-2010, 09:16 AM
RE: CaCl and RH correlation? - Ernesto - 01-26-2010, 11:49 AM
RE: CaCl and RH correlation? - CC Solutions - 01-27-2010 10:35 AM
RE: CaCl and RH correlation? - Ernesto - 01-27-2010, 12:56 PM
RE: CaCl and RH correlation? - eaadams - 07-09-2010, 11:56 AM
RE: CaCl and RH correlation? - mwoody - 08-31-2010, 10:34 AM
RE: CaCl and RH correlation? - eaadams - 08-31-2010, 10:47 AM